- plunger/piston(ceramic spraying)
- 2016-11-01 09:38
- wear resistant coatingPlasma spray (87%Al2O3+13%TiO2)Hardness (HV300=800)Porosity (2-4% dimension max 45m)Anchorage 3000
- Wire wheel(plasma spray)
- 2016-10-30 22:06
- wear resistant coatingPlasma spraing coating (99%Cr2O3)Hardness HV300=1200Surface Roughness: Ra0.4mAnchorage=3000psi
- Wire wheel(ceramic coating)
- 2016-10-24 17:34
- wear resistant coatingPlasma spraing coating (99%Cr2O3)Hardness HV300=1200Surface Roughness: Ra0.4mAnchorage=3000psi