Application: Used for welding ultra-low-carbon Cr19Ni10 stainless steel structures, and also used for 0Cr19Ni11Ti corrosion-resistant stainless steel structures whose working temperature is lower than 300 centi-degree. 0Cr19Ni11Ti corrosion-resistant stainless steel structures whose working temperature is lower than 300 centi-degree.
Attention:
1. It should be baked at 300-350 centi-degree for 1 hour before welding.
2. The weldment must be clear away impurities, such as oil, rust, moisture etc. Before welding.
3. Small current and short arc should be used in welding, and swaying broad lessthan 2.5 times of diameter of the electrode.
Chemical Compossition of Deposited metal(%)