Our amorphous diffusion alloy, brand 'Huida', is made by special temperature reduction and nano-materials. Ni reduced and nano-materials existed in amorphous shape formed by nano and sub-nano agglomeration. Ni based amorphous alloy will start to diffuse at over 300 temperature because that the surface active elements of nano, sub-nano, Ni based amorphous is more than carbonyl Ni powder and other forms distribution. And the diffusion speed will be enhanced by increasing temperature, to significantly improve the utilization efficiency of Ni and even dispersion in agglomerated materials, and reduce the sintering temperature and time of the products as well.
Generally, sintering temperature for electrolytic Ni powder is 1170 temperature-1200 temperature, for carbonyl Ni powder, 1150 temperature, while for amorphous diffusion alloy, 1120 temperature for 30-40min. It is added at -200 mesh, simple mixing process, not to affect the compressibility of Fe powder and has higher even dispersion.
By adding other nano-materials, and dispersing along the grain boundary in sintering process, to achieve dispersion strengthening, and then improve the strength, hardness and wear resistance of the products.