Our reclaimed rubber has Excellent aging properties, Minimum reversion, Reduced compound cost, Shorter breakdown in mixing time, Reduced power consumption, Lower processing temperature, Lower processing temperature, Lower processing temperature, Fast and uniform processing, Lower processing temperature, Improved dimensional stability.
Item Reclaimed rubber tires Reclaimed rubber galoshes Reclaimed Rubber sundry goods
Excellent First grade Qualified Excellent First grade First grade Qualified
Ashes% ≤ 10.00 12.00 15.00 32.00 38.00 30.00 40.00
Acetone-extract, % ≤ 20.00 25.00 28.00 17.00 19.00 20.00 25.00
Tensile Strength, MPa ≥ 9.50 8.00 6.00 5.50 4.00 5.50 4.50
Elongation break % ≥ 360 330 280 200 180 220 180
Mooney viscosity 70 75 80 80 80 70 80