Dimension: ??6, ??8, ??10, ??12, ??14, ??16, ??18, ??20, ??22, ??25, ??28, ??32, ??36, ??40
The technical data of Chinese standard ( Standard is GB1499, grade are HRB335, HRB400 and HRB500 ):
1. Chemical Composition
Carbon??0.25%; Si ??0.80%; Mn??1.60%; P??0.045%; S??0.045%;
Ceq: 0.52% for HRB335, 0.54% for HRB400, and 0.55% for HRB500.
V, Nb and Ti is allowed to add in the steel, N content is less than 0.012%
2. Mechanical composition:
Yield point: Min. 335 MPa for HRB335 grade, min 400 MPa for HRB400, and Min. 500 MPa for HRB500.
Tensile strength: Min. 490 MPa for HRB335 grade, min 570 MPa for HRB400, and Min. 630 MPa for HRB500.
3. Dimensional tolerance: Negotiable
4. The angle between transverse rib and axis is not less than 45 deg.
5. The transverse rib spacing is not more than 0.7 time of the bar's nominal diameter.
6. The angle between the side surface of transverse rib and the bar surface is not less than 45 deg.