Chemical & Physical Property of Cold Rolled Steel Coil
| Chemical Composition | C | Si | Mn | P | S |
| 0.04-0.05% | 0.01-0.02% | 0.18-0.22% | 0.014-0.016% | 0.006%-0.009% | |
| Yield Strength | (Mpa) 280-320 | ||||
| Tensile Strength | (Mpa) 340-390 | ||||
| Elongation | 23%-41% | ||||
Remarks of Product Storage
1. Store CR Coils in dry place free of dew and dampness.
2. During Storage, put wooden sleepers under the sheets as far as possible.
3. Provide waterproof covering for transportation and if any sheets are found wet on arrival, dry them immediately.
4. Handle material with care to avoid damage to edges, scratches or soiling on surface.
5. Use proper and suitable chemicals during fabrication to avoid erosion