Send Inquiry
COMPONENT: 40% MGO (Magnesia oxide)
35% MgCl2 (magnesium chloride)
15% FG (Fibreglass)
10% moisture (water)
ADVANTAGE
1, HIGH COMPRESSED FORCE
-- withstand 10, 000-12, 000psi (cement pot: Withstand only 2, 000psi)
-- LESS DAMAGE, LESS DUMPING EXPENSE
-- stackability in container or in warehouse
SAVE SPCE SAVE MONEY.
2, LIGHTER THAN TERRACOTTA AND CEMENT POT EQUIVALENTS
-- handle or move larger pots easier
3, CHEAPER THAN FIBRE GLASS OR POLY RESIN POT
4, HIHGER RESISTANCE AGAINST CHIPPING AND CRACKING
-- no chipping or product dust during handle or transport
5, WITHSTAND COLDER OR HOTTER TEMPERATURE
6, NATURE SURFACE / ENVIRonMENT FRIENDLY
Package: Stackability in container