Send Inquiry
This line is mainly used to produce PP staple fiber from the PP chips. The finished product is PP staple fiber of 1.5 Den. to 15 Den. Technical Process
Pneumatic Raw Material Conveyer—Hopper—Filter—Melt Pipe—Spin Beam—Meter Pump—Spinning—Cooling Solidification—Oiling—Tow Guide—Stretcher—Hot Air—Stretcher—Stacker—Crimper& Oiling—Relaxing Heat Oven—Tow Guide Stand—Tension Device—Cutter—Pneumatic Conveyer—Baler
Main Technical Parameter
1. Screw Extruder: 1 set×2
2. Spinning Position: 6 ×2
3. Distance Between Adjacent Spinning Positions: 1100mm
4. Hole No. of Spinneret: 52008 holes for 1.5 D-4D spinneret; 4.5D-7D 28000 holes
5. Hole Type of Spinneret: Circular
6. Spinning Speed: 20-70M/min
7. Drawing Speed: 150M/min
8. Draft Total Denier: 2500000D (Max)
Welcome to contact us with detailed information.